Sichuan Shimian Mine Concentrator

Asbestos mine in Sichuan Province County, built a roughing station and three beneficiation plants. The ore mined in the underground is crushed by the roughing station-hand selection-screening process. After pre-concentration, it is supplied to the first and second concentrating plants, and the open-pit mining ore is directly supplied to the third concentrating plant.
The length of the asbestos fiber in the ore is 0.5~10mm, the maximum size of the underground ore is 400mm, the moisture is 4%~6%, and the grade is 1.0%~2.5%.
The process and equipment of the three concentrators of the mine are basically the same, and the process flow of the second workshop of the first plant is shown in the following figure. In the process, the three-stage crushing and uncovering cotton is used, and the impact crusher , the vertical shaft hammer crusher and the cage crusher are respectively used, and the three-stage sorting adopts the plane rotary sieve and the plane shaking sieve suction selection, and the coarse fine cotton selected in each section is selected. The three streams are divided into hexagonal sieves and small flat sieves for dust removal and sand removal. Drying is carried out using a cylinder dryer. The first stream produces long cotton (Class II), the second stream produces medium long cotton (Class III-IV), and the third stream produces short cotton (Grade V).

The design capacity of the mine is 15000t/a, the mine has a grain size of 500mm, the ore grade is 1.38%, and the ore water is 5.08%. The size of the ore in the selected workshop is 50mm, the selected grade is 2.42%, and the moisture in the selection is 2.00%. The grade of tailings is 0.5%, the grade of tailings is 0.31%, the recovery rate of ore is 90.31%, and the yield of Grade IV or above is 15.19%.

Barbed Wire

The barbed wire is twisted and braided by a fully automated barbed wire machine. Commonly known as tribulus terrestris, barbed wire, and barbed thread among the people. Finished product types: single-filament twisted and double-filament twisted.
Raw materials: high-quality low-carbon steel wire.
Surface treatment process: electro-galvanized, hot-dip galvanized, plastic-coated, spray-coated. There are blue, green, yellow and other colors.
The reason for surface treatment is to enhance the anti-corrosion strength and prolong the service life. As the name suggests, the surface treatment of galvanized barbed wire is galvanized, which can be electro-galvanized or hot-dip galvanized; the surface treatment of PVC barbed wire is PVC-coated, and the barbed wire inside is black wire, electroplated wire and hot-dip galvanized wire.
Uses: Used for the isolation and protection of grassland borders, railways, and highways.


Barbed Wire 4Barbed Wire 13



Barbed Wire,Anti-Climb Blade Barbed Wire,Galvanized Security Fencing Barbed Wire,Hot Dipped Galvanized Barbed Wire

Anping County Dongjie Wiremesh Products Co., Ltd. , https://www.dongjiewiremesh.com